... | ... | @@ -8,8 +8,15 @@ When the sample shape is too complex so that a backing mold cannot be made to [c |
|
|
|
|
|
https://www.nature.com/articles/s41598-017-11433-4
|
|
|
|
|
|
https://formlabs.com/fr/3d-printers/form-2/
|
|
|
https://www.stratasys.com/
|
|
|
https://www.stratasys.com/materials/search/veroclear
|
|
|
|
|
|
stratasys VeroClear but large modulus quite expensive
|
|
|
other like stereolito poorly transparent and photoelastic
|
|
|
other like stereolito poorly transparent and photoelastic material quite brittle good only for 'rapid' prototyping
|
|
|
|
|
|
![IMG_9795.resized](uploads/82a211c688ce57adbbbd40a103cd0657/IMG_9795.resized.JPG)
|
|
|
![IMG_9794.resized](uploads/736551685e78a101572e520c06308195/IMG_9794.resized.JPG)
|
|
|
|
|
|
make 3D shape not always reachable with molding processes
|
|
|
|
... | ... | |